Home > Products > Stainless Steel Pipe > GB/T12770 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures

GB/T12770 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures

Payment Type:
L/C,T/T,D/P,Paypal,Money Gram,Western Union
Incoterm:
FOB,CFR,CIF,FCA,CPT
Min. Order:
5 Ton
Transportation:
Ocean,Land,Air
Port:
Ningbo,Shanghai,Zhoushan
Share:
Chat Now
  • Product Description
Overview
Product Attributes

Model No.GB/T12770

BrandTorich

TypeWelded

CertificationUL

ApplicationStructure Pipe

Section ShapeRound

Surface TreatmentPolished

UsageConstruction & Decoration

TechniqueCold Rolled Cold Drawn

MaterialStainless Steel 201/304/316

FinishHeat Treatment

WT0.5-50mm

NameGB/T12770 Material 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes For Mechanical Structures

GradeS30210 S30408 S30403 S31008

SurfacePickling,polished

OD3-500mm

Supply Ability & Additional Information

Packagingin seaworthy packing

Productivity50000tons/year

TransportationOcean,Land,Air

Place of OriginZhejiang, China (Mainland)

Supply Ability60000 Ton per year

CertificateISO9001:2008 ISO14001:2008, TS16949, CE PED, TUV, API

HS Code7306110000

PortNingbo,Shanghai,Zhoushan

Payment TypeL/C,T/T,D/P,Paypal,Money Gram,Western Union

IncotermFOB,CFR,CIF,FCA,CPT

Packaging & Delivery
Selling Units:
Ton
Package Type:
in seaworthy packing

Product Name: GB/T12770 Material 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures

 

Size range: O.D.:3-500mm W.T.:0.5-50mm L:2000-12000mm according to customers' actual application and production.

 

Application : For Mechanical Structures purposes

 

Steel Grade: 12Cr18Ni9,06Cr19Ni10,022Cr19Ni10,06Cr25Ni20,022Cr22Ni5Mo3N,019Cr19Mo2NbTi,06Cr13Al

 

Characteristic:

Good concentricity

Good surface quality

Good OD and ID tolerance

High Precision

Stable quality

Smooth Roughness

TORICH QUALITY ASSURANCE

 

Table1Tolerance of OD

Classification Nominal OD Permissible Tolerance
PC PB PA

H

T

<25 ±0.20 ±0.15 ±0.10
≥25~<40 ±0.30 ±0.25 ±0.20
≥40~<63 ±0.50 ±0.30 ±0.25
≥63~<90 ±0.60 ±0.50 ±0.40
≥90~<159 ±0.80 ±0.65 ±0.50
≥159~<300 ±0.8%D ±0.7%D ±0.5%D
≥300~<610 ±0.1%D ±0.8%D ±0.6%D
≥10 protocol protocol protocol

WC

SP

<25 ±0.15 ±0.12 ±0.10
≥25~<40 ±0.20 ±0.15 ±0.13
≥40~<50 ±0.20 ±0.18 ±0.15
≥50~<60 ±0.25 ±0.20 ±0.18
≥60~<90 ±0.30 ±0.28 ±0.25
≥90~<100 ±0.40 ±0.35 ±0.30
≥100~<200 ±0.5%D ±0.4%D protocol
≥200 protocol protocol protocol

Table 2Tolerance of WT

Nominal WT Permissible Tolerance
<0.5 ±0..10
≥0.5~1.0 ±0.15
>1.0~2.0 ±0.20
>2.0~<4.0 ±0.30
≥4.0 ±10%S

 

Table 3 Bending Degree

Nominal Wall Thickness/mm Bending Degree/(mm/m)
≤108 ≤1.0
>108~325 ≤1.5
>325 ≤2.5

 

Table4 The density of the steel and Calculation of Theoretic Weight

No. Steel Grade Density/(kg/dm3) The formula after conversion
1 12Cr18Ni9 7.93 W=0.02491S(D-S)
2 06Cr19Ni10
3 022Cr19Ni10 7.90 W=0.02482S(D-S)
4 06Cr25Ni20 7.98 W=0.02507S(D-S)
5 06Cr17Ni12Mo2 8.00 W=0.02513S(D-S)
6 022Cr17Ni12Mo2
7 06Cr18Ni11Ti 8.03 W=0.02523S(D-S)
8 06Cr18Ni11Nb
9 022Cr22Ni5Mo3N 7.80 W=0.02450S(D-S)
10 022Cr23Ni5Mo3N
11 022Cr25Ni7Mo4N
12 022Cr18Ti 7.70 W=0.02491S(D-S)
13 019Cr19Mo2NbTi 7.75 W=0.02435S(D-S)
14 06Cr13Al
15 022Cr11Ti
16 022Cr12Ni
17 06Cr13

 

Table 5 Steel Grade and Chemical Componenet

No. Type Unified digital code Grade Chemical Componenet(Quality Fraction)/%
C Si Mn P S Ni Cr Mo N Others
1 Austenite S30210 12Cr18Ni9 ≤0.15 ≤0.75 ≤2.00 ≤0.040 ≤0.030 8~10 17~19 - ≤0.10 -
2 S30408 06Cr19Ni10 ≤0.08 ≤0.75 ≤2.00 ≤0.040 ≤0.030 8~11 18~20 - - -
3 S30403 022Cr19Ni10 ≤0.030 ≤0.75 ≤2.00 ≤0.040 ≤0.030 8~12 18~20 - - -
4 S31008 06Cr25Ni20 ≤0.08 ≤1.50 ≤2.00 ≤0.040 ≤0.030 19~22 24~26 - - -
5 S31608 06Cr17Ni12Mo2 ≤0.08 ≤0.75 ≤2.00 ≤0.040 ≤0.030 10~14 16~18 2~3 - -
6 S31603 022Cr17Ni12Mo2 ≤0.08 ≤0.75 ≤2.00 ≤0.040 ≤0.030 10~14 16~18 2~3 - -
7 S32168 06Cr18Ni11Ti ≤0.08 ≤0.75 ≤2.00 ≤0.040 ≤0.030 9~12 17~19 - - Ti15C~0.70
8 S34778 06Cr18Ni11Nb ≤0.08 ≤0.75 ≤2.00 ≤0.040 ≤0.030 9~12 17~19 - - Nb110C~1010
9 Bipolar S22253 022Cr22Ni5Mo3N ≤0.030 ≤1.00 ≤2.00 ≤0.030 ≤0.020 4.5~6.5 21~23 2.5~3.5 0.08~0.20  
10 S22053 022Cr23Ni5Mo3N ≤0.030 ≤1.00 ≤2.00 ≤0.030 ≤0.020 4.5~6.5 22~23 3~3.5 0.14~0.20  
11 S25073 022Cr25Ni7Mo4N ≤0.030 ≤0.80 ≤1.20 ≤0.035 ≤0.020 6~8 24~26 3~5 0.24~0.32 Cu≤0.50
12 Ferrite S11863 022Cr18Ti ≤0.03 ≤0.75 ≤1 ≤0.04 ≤0.03 (0.60) 16~19 - - Ti or Nb:0.1~1
13 S11972 019Cr19Mo2NbTi ≤0.025 ≤0.75 ≤1 ≤0.04 ≤0.03 1.00 17.5~19.50 1.75~2.50 ≤0.035 (Ti+Nb):[0.2+4(C+N)]~0.8
14 S11348 06Cr13Al ≤0.08 ≤0.75 ≤1 ≤0.04 ≤0.03 (0.60) 11.50~14.50 - - Al:0.1~0.3
15 S11163 022Cr11Ti ≤0.03 ≤0.75 ≤1 ≤0.04 ≤0.02 (0.60) 10.50~11.70 - ≤0.030 Ti≥8(C+N),Ti:0.15~0.50,Nb≤0.10
16 S11213 022Cr12Ni ≤0.03 ≤0.75 ≤1.5 ≤0.04 ≤0.015 0.3~1.00 10.50~12.50 - ≤0.030  
17 Martensitic S41008 06Cr13 ≤0.08 ≤0.75 ≤1 ≤0.04 ≤0.03 (0.60) 11.50~13.50 - - -
Note:The number in brackets is the maximum allowed to be added. Chemical component of some grade is different from GB/T20878.

 

 

Table 6 Recommendatory heat treating regime of the steel tubes

No. Type Steel grade Recommendatory heat treating regime
1 Austenite 12Cr18Ni9 1010℃~1150℃,water-cooling or other methods of rapid cooling
2 06Cr19Ni10 1010℃~1150℃,water-cooling or other methods of rapid cooling
3 022Cr19Ni10 1010℃~1150℃,water-cooling or other methods of rapid cooling
4 06Cr25Ni20 1030℃~1180℃,water-cooling or other methods of rapid cooling
5 06Cr17Ni12Mo2 1010℃~1150℃,water-cooling or other methods of rapid cooling
6 022Cr17Ni12Mo2 1010℃~1150℃,water-cooling or other methods of rapid cooling
7 06Cr18Ni11Ti 920℃~1150℃,water-cooling or other methods of rapid cooling
8 06Cr18Ni11Nb 980℃~1150℃,water-cooling or other methods of rapid cooling
9 Dual-phase steel 022Cr22Ni5Mo3N 1020℃~1100℃,water-cooling
10 022Cr23Ni5Mo3N 1020℃~1100℃,water-cooling
11 022Cr25Ni7Mo4N 1025℃~1125℃,water-cooling
12 Ferritic 022Cr18Ti 780℃~950℃,rapid cooling or slow cooling
13 019Cr19Mo2NbTi 800℃~1050℃,rapid cooling
14 06Cr13Al 780℃~830℃,rapid cooling or slow cooling
15 022Cr11Ti 800℃~900℃,rapid cooling or slow cooling
16 022Cr12Ni 700℃~820℃,rapid cooling or slow cooling
17 Martensite 06Cr13 750℃,rapid cooling ;800℃~900℃,slow cooling



Welded Stainless Steel Tubes


China Stainless Steel Tube manufacturers, our Stainless Steel Exhaust Tube, Welded Steel Tube, Round Stainless Steel Pipe, Polish Stainless Steel Tube, Stainless Coiled Tube, Duplex Stainless Steel Tube are good in quality and competitive in price.

Product Categories : Stainless Steel Pipe

Home > Products > Stainless Steel Pipe > GB/T12770 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures
Email to this supplier
  • *Subject:
  • *To:
    Mr. Richard SHEN
  • *Email:
  • *Message:
    Your message must be between 20-8000 characters
Send Inquiry
*
*

Related Products List

Home

Product

Whatsapp

About Us

Inquiry

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send